Differential scanning calorimetry of polysulfone at high pressures of CO2 and N2O

✍ Scribed by Yasuhisa Kishimoto; Ryo Ishii


Book ID
106002607
Publisher
Springer
Year
1999
Tongue
English
Weight
213 KB
Volume
43
Category
Article
ISSN
0170-0839

No coin nor oath required. For personal study only.