Differential Scanning Calorimetry Cure Studies of Tetra-N-glycidyldiaminodiphenylmethane Epoxy Resins Part 2 - Reaction with 4,4′-Diaminodiphenylsulphone Accelerated by Borontriofluoride-Ethylamine

✍ Scribed by Barton, John M.


Publisher
Wiley (John Wiley & Sons)
Year
1986
Tongue
English
Weight
506 KB
Volume
18
Category
Article
ISSN
0007-1641