✦ LIBER ✦
Differential scanning calorimetry applied to cross-linking of a filled epoxy resin: Accuracy of the Borchardt and Daniels equation for describing the curing process kinetics
✍ Scribed by L. Elegant; P. Tomi; G. Augier; J. P. Nicolas; G. Pecqueux
- Publisher
- Springer Netherlands
- Year
- 1986
- Tongue
- English
- Weight
- 359 KB
- Volume
- 31
- Category
- Article
- ISSN
- 0022-5215
No coin nor oath required. For personal study only.