✦ LIBER ✦
Differential scanning calorimetric studies on As–Te–Si glasses: Network topological effects and the composition dependence of thermal parameters
✍ Scribed by M. Anbarasu; S. Asokan
- Book ID
- 116669343
- Publisher
- Elsevier Science
- Year
- 2006
- Tongue
- English
- Weight
- 123 KB
- Volume
- 352
- Category
- Article
- ISSN
- 0022-3093
No coin nor oath required. For personal study only.