Differential scanning calorimeter and infrared imaging for electrocaloric characterization of poly(vinylidene fluoride-trifluoroethylene-chlorofluoroethylene) terpolymer
✍ Scribed by Sebald, Gael; Seveyrat, Laurence; Capsal, Jean-Fabien; Cottinet, Pierre-Jean; Guyomar, Daniel