𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Dielectric and physico-mechanical properties of butyl rubber loaded with some white fillers

✍ Scribed by Hanna, Faika F. ;Yehia, Abbas A. ;Hakim, Itedal K. ;Bishai, Augenie M. ;Saad, Azima L. G.


Publisher
Wiley (John Wiley & Sons)
Year
1983
Tongue
English
Weight
186 KB
Volume
15
Category
Article
ISSN
0007-1641

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Electrical and mechanical properties of
✍ A. F. Younan; S. L. Abd-El-Messieh; A. A. Gasser πŸ“‚ Article πŸ“… 1998 πŸ› John Wiley and Sons 🌐 English βš– 159 KB πŸ‘ 2 views

The permittivity Ј and dielectric loss Π‰ for different ratios of an ethylene propylene diene monomer (EPDM)-chloroprene rubber (CR) blend ranging from 0 to 100 phr were measured over a frequency range from 400 Hz to 60 kHz. The measurements were carried out at room temperature (25Β°C). The values of

Dielectric relaxation and mechanical pro
✍ S. L. Abd-El-Messieh; A. F. Younan πŸ“‚ Article πŸ“… 1996 πŸ› John Wiley and Sons 🌐 English βš– 555 KB

A systematic dielectric study over a frequency range from 400 to 10 MHz was carried out on natural rubber and chloroprene rubber with a small amount of nitroaniline additives. Three absorption regions were obtained as a result of the analysis of the curves relating dielectric loss k with frequency.

Some factors affecting the electrical pr
✍ E. M. Abdel-Bary; H. H. Hassan; A. M. El-Lawindy; M. K. Abu-Assy; F. K. El-Tanta πŸ“‚ Article πŸ“… 1993 πŸ› John Wiley and Sons 🌐 English βš– 285 KB

## Abstract Butyl rubber mixtures loaded with 70 phr general purpose furnace black (GPF) and tetramethyl thiuram disulphide (TMTD)/S as vulcanizing system were prepared. The kinetics of their electrical conductivity development during the vulcanization process were followed by using an especially d