The hot deformation characteristics of a Ni-base superalloy are studied in the temperature range 1000-1200 Β°C and strain rate range 0.001-1.0 s Γ1 using hot compression tests. Processing maps for hot working are developed on the basis of the variations of efficiency of power dissipation with tempera
β¦ LIBER β¦
Development of processing maps for a Ni-based superalloy
β Scribed by Dayong Cai; Liangyin Xiong; Wenchang Liu; Guidong Sun; Mei Yao
- Book ID
- 113780050
- Publisher
- Elsevier Science
- Year
- 2007
- Tongue
- English
- Weight
- 911 KB
- Volume
- 58
- Category
- Article
- ISSN
- 1044-5803
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Characterization of hot deformation beha
β
Dayong Cai; Liangyin Xiong; Wenchang Liu; Guidong Sun; Mei Yao
π
Article
π
2009
π
Elsevier Science
β 749 KB
Development of Ni-based superalloys for
β
Devin E. Burns; Yong Zhang; Michael Teutsch; Klaus Bade; Jarir Aktaa; Kevin J. H
π
Article
π
2012
π
Elsevier Science
π
English
β 668 KB
Development of a diffusion mobility data
β
C.E Campbell; W.J Boettinger; U.R Kattner
π
Article
π
2002
π
Elsevier Science
π
English
β 198 KB
Processing maps for Feβ24Niβ11Crβ3Tiβ1Mo
β
CAI DAYONG; ZHANG CHUNLING; TANG ZHIGUO; DONG HAIFENG; WANG PENG
π
Article
π
2011
π
Springer-Verlag
π
English
β 382 KB
Development of a low-expansion bond coat
β
Klaus Fritscher; Christoph Leyens; Manfred Peters
π
Article
π
1995
π
Elsevier Science
π
English
β 550 KB
Ternary NiCrAI alloys were modified by the addition of Ti and Si in order to adjust their coefficients of thermal expansion (CTE) to less than 15 x 10 -6 K -j (from room temperature to 1000 Β°C) without sacrificing essential high temperature oxidation resistance. Vacuum induction melted cast alloy sa
Life prediction of a Ni-base superalloy
β
M AGHAIE-KHAFRI; M NOORI
π
Article
π
2011
π
Springer-Verlag
π
English
β 318 KB