Development of pitting corrosion on 20Kh13 steel

✍ Scribed by K. V. Rybalka; L. A. Beketaeva; V. S. Shaldaev; L. V. Kasparova; A. D. Davydov


Book ID
110202080
Publisher
SP MAIK Nauka/Interperiodica
Year
2009
Tongue
English
Weight
573 KB
Volume
45
Category
Article
ISSN
1023-1935