๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Development of Ir-base refractory superalloys

โœ Scribed by Y. Yamabe; Y. Koizumi; H. Murakami; Y. Ro; T. Maruko; H. Harada


Book ID
116175793
Publisher
Elsevier Science
Year
1996
Tongue
English
Weight
458 KB
Volume
35
Category
Article
ISSN
1359-6462

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


New developed quaternary refractory supe
โœ Xihong Yu; Yoko Yamabe-Mitarai; Yoshikazu Ro; Hiroshi Harada ๐Ÿ“‚ Article ๐Ÿ“… 2000 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 553 KB