๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Determination of Rubber Hydrocarbon by Gravimetric Rubber Bromide Method

โœ Scribed by Willits, C.O.; Swain, M.L.; Ogg, C.L.


Book ID
126838603
Publisher
American Chemical Society
Year
1946
Weight
602 KB
Volume
18
Category
Article
ISSN
0096-4484

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


The direct determination of India rubber
โœ John B. Tuttle; Louis Yurow ๐Ÿ“‚ Article ๐Ÿ“… 1919 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 41 KB

## 693 showed that there was no marked difference in the behavior o,f the three alloys in the test although the E series was somewhat superior and the G series somewhat inferior to the others. All of the three alloys will withstand IO,OOO,OOO complete reversals (tension to compression) at a maximu

Diffusion of hydrocarbons in rubber, mea
โœ E. Von Meerwall; R. D. Ferguson ๐Ÿ“‚ Article ๐Ÿ“… 1979 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 792 KB

## Abstract The pulsed field gradient spin echo method was used to measure the diffusion of ten paraffin hydrocarbons in several uncrosslinked rubbers at 51ยฐC. We obtain various free volume parameters from the concentration dependences, establish the approximate proportionality of the translational