Determination of optimum compatibilizer (SMA) concentration for PBT/ABS (70/30) blend using tensile strength data

✍ Scribed by Diya Basu; Amarnath Banerjee


Publisher
John Wiley and Sons
Year
1997
Tongue
English
Weight
97 KB
Volume
64
Category
Article
ISSN
0021-8995

No coin nor oath required. For personal study only.

✦ Synopsis


Poly(butylene terephthalate) (PBT), a thermoplastic polyester, was melt blended with acrylonitrile-butadiene-styrene (ABS) terpolymer using styrene-maleic anhydride (SMA) as the compatibilizer. The PBT : ABS ratio was fixed at 70 : 30 by weight and weight percent (wt %) of SMA was varied as 2.5, 5, and 7.5. The effect of variation of the SMA percent in the blend was studied by calculating and comparing the theoretical tensile strength values with the experimental ones. The adhesive strength (s) and the interaction parameter ( I) were also determined.