Determination of Ca(OH)2 in hydrated cement paste by differential scanning calorimetry

✍ Scribed by M. Moukwa; S. Farrington; D. Youn


Publisher
Elsevier Science
Year
1992
Tongue
English
Weight
460 KB
Volume
195
Category
Article
ISSN
0040-6031