Determination of Aluminum in Nickel-Based Superalloys by Using Laser-Induced Breakdown Spectroscopy

✍ Scribed by Zhu, Dehua; Wang, Xi; Ni, Xiaowu; Chen, Jianping; Lu, Jian


Book ID
124087475
Publisher
IOP Publishing
Year
2011
Tongue
English
Weight
773 KB
Volume
13
Category
Article
ISSN
1009-0630

No coin nor oath required. For personal study only.