Detection of the liquid — liquid demixing by differential scanning calorimetry

✍ Scribed by Eugeniusz Maderek; B. A. Wolf


Publisher
Springer
Year
1983
Tongue
English
Weight
308 KB
Volume
10
Category
Article
ISSN
0170-0839

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Some evidence against the existence of t
✍ Chen, J. ;Kow, C. ;Fetters, L. J. ;Plazek, D. J. 📂 Article 📅 1982 🏛 Wiley (John Wiley & Sons) 🌐 English ⚖ 958 KB

## Abstract The liquid‐liquid transition __T__~ll~ has been examined by using differential scanning calorimetry as the tool of measurement. The results presented show that for the case of polystyrene, the __T__~ll~ event appears to be an artifact caused by the presence of volatile components. Purif