Using specimens of western hemlock with various depths, double cantilever beam and three-point bend end-notched flexure tests were conducted to obtain the mode I and mode II fracture toughness. To correct the deflection caused by shearing and crack tip deformation, four conventional data reduction m
โฆ LIBER โฆ
Delamination characteristics of double-cantilever beam and end-notched flexure composite specimens
โ Scribed by C.T. Sun; S. Zheng
- Publisher
- Elsevier Science
- Year
- 1996
- Tongue
- English
- Weight
- 979 KB
- Volume
- 56
- Category
- Article
- ISSN
- 0266-3538
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Shear and crack tip deformation correcti
โ
Hiroshi Yoshihara; Akihiko Satoh
๐
Article
๐
2009
๐
Elsevier Science
๐
English
โ 704 KB
Mode I and mode II initiation fracture t
โ
Hiroshi Yoshihara
๐
Article
๐
2010
๐
Elsevier Science
๐
English
โ 879 KB
Using specimens of medium density fiberboard, double cantilever beam and three-point bend end-notched flexure tests were conducted to obtain the mode I and mode II initiation fracture toughness and resistance curve for in-plane and through-the-thickness systems. The mode I initiation fracture toughn