Degradation of nylon-6 in ethylene glycol: 2. Mathematical illustration of degradation
β Scribed by P Huczkowski; J Kapko
- Publisher
- Elsevier Science
- Year
- 1980
- Tongue
- English
- Weight
- 210 KB
- Volume
- 21
- Category
- Article
- ISSN
- 0032-3861
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Abstract Peroxide radical concentrations were measured from both PET and nylon 6 fibers mechanically stretched in air at room temperature and quickly quenched into liquid nitrogen. The radical concentrations depend on degree of stretching as well as conditions under which the fibers were made, i
The degradation of poly(propylene fumarate-coethylene glycol) hydrogels was examined in vitro in phosphate-buffered saline at pH 7.4 and in vivo in a subcutaneous rat model. These hydrogels have potential application as biodegradable, injectable cardiovascular stents, and, as such, their mass loss,