๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Crystalline morphology of ultrahigh-molecular-weight polyethylene pseudogels

โœ Scribed by Anagnostis E. Zachariades


Publisher
John Wiley and Sons
Year
1986
Tongue
English
Weight
659 KB
Volume
32
Category
Article
ISSN
0021-8995

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Morphology of chemically crosslinked ult
โœ Shen, F.-W. ;McKellop, H. A. ;Salovey, R. ๐Ÿ“‚ Article ๐Ÿ“… 1998 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 757 KB

Morphological characterization of chemically crosslinked ultrahigh molecular weight polyethylene was performed by differential scanning calorimetry and scanning electron microscopy. The lamellar thickness of nascent UHMWPE inferred from DSC endotherms showed a very broad distribution, which was redu

Processing of ultrahigh molecular weight
โœ Xi-You Wang; Sheng-Ying Li; R. Salovey ๐Ÿ“‚ Article ๐Ÿ“… 1988 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 394 KB ๐Ÿ‘ 2 views

The extent of recrystallization of nascent UHMWPE powder is easily measured by calorimetry. Melting and recrystallization of nascent UHMWPE at 140ยฐC can be suppressed by compression molding. Crystals of UHMWPE prepared from dilute solution show a peak melting temperature of 140ยฐC and exhibit crystal

Dynamic thermomechanical properties and
โœ Lewis, Gladius ;Rogers, Christopher ;Trieu, Hai H. ๐Ÿ“‚ Article ๐Ÿ“… 1998 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 299 KB ๐Ÿ‘ 2 views

A dynamic thermomechanical analysis method was used to determine the values of the viscoelastic parameters, storage modulus (E) and the tangent of the loss angle (tan d) of samples taken from the near surface and core regions of ultrahigh molecular weight polyethylene (UHMWPE) bar stock specimens th

Roller drawing of ultrahigh molecular we
โœ Akira Kaito; Kazuo Nakayama; Hisaaki Kanetsuna ๐Ÿ“‚ Article ๐Ÿ“… 1985 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 922 KB

The roller drawing of ultrahigh molecular weight polyethylene (UHMW-PE) sheets were carried out in the roller temperature T, range of 100-140ยฐC. In addition to the roller drawing in the solid state (T, = lOOT), we attempted to crystallize the molten UHMW-PE sheet under the rollerdrawing process (T,