Laser crystal Nd:CaNb 2 O 6 with excellent quality has been grown by Czochralski technique. The effective segregation coefficient of Nd 3+ was studied by X-ray fluorescence method. The polarized absorption spectra and the fluorescence spectra of Nd:CaNb2O6 were measured at room temperature. The peak
Crystal growth, optical properties, and continuous-wave laser operation of Nd3+-doped Lu2SiO5 crystal
β Scribed by D.Z. Li; X.D. Xu; D.H. Zhou; C.T. Xia; F. Wu; J. Xu; Z.H. Cong; J. Zhang; D.Y. Tang
- Publisher
- John Wiley and Sons
- Year
- 2010
- Tongue
- English
- Weight
- 223 KB
- Volume
- 8
- Category
- Article
- ISSN
- 1612-2011
No coin nor oath required. For personal study only.
β¦ Synopsis
High quality Nd 3+ -doped Lu 2 SiO 5 (Nd:LSO) crystal has been grown by the Czochralski technique. The cell parameters were analyzed with X-ray diffraction (XRD). Room temperature absorption and fluorescence spectra and fluorescence lifetime of the Nd:LSO crystal were measured and analyzed. The Judd-Ofelt intensity parameters Ξ© 2,4,6 were obtained to be 2.59, 4.90, and 5.96Γ10 -20 cm 2 , respectively. The absorption and emission cross sections and the branching ratios were calculated. The peak emission cross section is 5.8 and 6.6Γ10 -20 cm 2 at 1075 and 1079 nm, respectively, with full width at half maximum (FWHM) of 2.8 and 5.1 nm in turn. Pumped by a laser diode, a maximum 2.54 W continuous-wave laser output has been obtained with a slope efficiency of 32%. All the results show that this crystal is a promising laser material.
Output power, W 2.0 2.5 1.0 1.
π SIMILAR VOLUMES
In this paper, the crystal growth and characterization of Nd:Gd3AlxGa5-xO12 (x = 0.94) (Nd:GGAG) was reported. The X-ray powder diffraction studies confirm that the Nd:Gd 3 Al x Ga 5-x O 12 crystal is isostructural with Gd 3 Ga 5 O 12 (GGG) with unit cell parameter of 1.2319 nm. The absorption and e
Diode pumped continuous wave operation and passively Q-switched performances of a Nd:Sc2SiO5 laser crystal at 1.08 microns have been demonstrated. A maximum continuous wave average output power up to 1.86 W has been obtained, corresponding to an optical conversion efficiency of 20.7% and a slope eff
## Abstract In:Fe:LiTaO~3~ crystals were grown in an air atmosphere using the Czochralski method. The photorefractive properties were measured by the twoβwave coupling experiments, and lightβinduced scattering was used to characterize the optical damage. It was found that the photorefractive respon