Highly c-axis oriented (Tl 0.5 ,Pb 0.5 )(Sr 0.8 ,Ba 0.2 ) 2 Ca 2 Cu 3 O y films with a thickness of 1.5 lm and 4 lm were prepared by screen printing method on untextured silver substrates. Tl-1223 films have the critical temperatures around 116 K with transition widths, DT, of 2 K, The microstructur
✦ LIBER ✦
Critical currents of (Tl0.5Pb0.5)(Sr0.85Ba0.15)2Ca2Cu3Oz films on untextured silver substrates
✍ Scribed by W.M. Woch; R. Zalecki; A. Kołodziejczyk; C. Deinhofer; G. Gritzner
- Book ID
- 116601568
- Publisher
- Elsevier Science
- Year
- 2007
- Tongue
- English
- Weight
- 467 KB
- Volume
- 442
- Category
- Article
- ISSN
- 0925-8388
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Microstructure of screen-printed (Tl0.5,
✍
Bong-Jun Kim; Hyun-Tak Kim; Yoshio Matsui; Dae-Yong Jeong; Christian Deinhofer;
📂
Article
📅
2007
🏛
Elsevier Science
🌐
English
⚖ 225 KB
Study of critical current density in (Tl
✍
M.F. Tai; Y.K. Tu; I.C. Jou
📂
Article
📅
1990
🏛
Elsevier Science
🌐
English
⚖ 320 KB
K and has a logarithmic temperature dependence below 40 K. An anomalous dimpling behavior occurs near the origin of the loop for powder sample. This Je decreases slightly with magnetic field at low temperature and reaches a stable value at high field. The flux pinning centers may be considered as co
XANES and EXAFS study of (Tl0.5Pb0.5)Sr2
✍
Zając, D.A.; Woch, W.M.; Stępień, J.; Kapusta, Cz.; Kołodziejczyk, A.; Sudra, H.
📂
Article
📅
2013
🏛
Elsevier Science
🌐
English
⚖ 433 KB
High critical current densities in (Tl0.
✍
P. Pugnat; K. Lebbou; M. T. Cohen-Adad; J. L. Jorda; M. Couach; G. Fillion
📂
Article
📅
1996
🏛
Springer
🌐
English
⚖ 156 KB
Phase diagram for (Tl0.5Pb0.5)(Ba0.2Sr0.
✍
F.L. Stavale; J.L. Gonzalez; E.S. Yugue; E. Baggio-Saitovitch
📂
Article
📅
2004
🏛
Elsevier Science
🌐
English
⚖ 272 KB
Effect of Te Substitution on (Tl0.5Pb0.5
✍
Yusrianto, Efil; Abd-Shukor, R.
📂
Article
📅
2012
🏛
Springer
🌐
English
⚖ 567 KB