๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Creep of CMSX-4 superalloy single crystals: effects of rafting at high temperature

โœ Scribed by R.C Reed; N Matan; D.C Cox; M.A Rist; C.M.F Rae


Publisher
Elsevier Science
Year
1999
Tongue
English
Weight
384 KB
Volume
47
Category
Article
ISSN
1359-6454

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


A model for the creep deformation behavi
โœ A. Ma; D. Dye; R.C. Reed ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 385 KB

Constitutive equations are constructed for single-crystal nickel-based superalloys. Account is taken of dislocation glide in the channels of the matrix phase (referred to as c) of the face-centred cubic (fcc) type, dislocation climb at the interfaces with the reinforcing L1 2 precipitates (referred

Shear Creep Deformation of the Super All
โœ M. Kamaraj; K. Serin; M. Kolbe; K. Neuking; G. Eggeler ๐Ÿ“‚ Article ๐Ÿ“… 2003 ๐Ÿ› John Wiley and Sons ๐ŸŒ English โš– 592 KB

## Abstract In the present paper we investigate the shear creep behavior of the single crystal super alloy CMSXโ€4 at temperatures between 950 and 1100โ€ŠยฐC and shear stresses ranging from 80 to 155 MPa. A double shear creep test technique is used to study the shear creep behavior of four specific mac

Anisothermal creep behavior at very high
โœ J. Cormier; X. Milhet; J. Mendez ๐Ÿ“‚ Article ๐Ÿ“… 2008 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 438 KB

Nickel-based superalloy single crystal specimens have been tested under anisothermal creep conditions using two different routes, both including an overheating stage. In the first route, the material is tested under creep conditions at 1050 โ€ข C, then submitted to an overheating regime at 1200 โ€ข C, a