𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Corrosion and stress corrosion cracking behavior of equal channel angular pressed oxygen-free copper in 3.5% NaCl solution

✍ Scribed by Y. H. Jang; S. S. Kim; S. Z. Han; C. Y. Lim; C. J. Kim


Publisher
Springer
Year
2006
Tongue
English
Weight
715 KB
Volume
41
Category
Article
ISSN
0022-2461

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


An investigation of Stress corrosion cra
✍ Dr. A. Moccari; C. R. Shastry πŸ“‚ Article πŸ“… 1979 πŸ› John Wiley and Sons 🌐 English βš– 565 KB

## Abstract Effect of specimen orientation, heat treatment and applied potential on the stress corrosion susceptibility of magnesium AZ61 (Mg‐6.3% Al‐0.5% Zn‐0.20% Mn) alloy in an aqueous 3.5% NaCl + 2% K~2~CrO~4~ solution at room temperature was investigated. Stress corrosion times to failure were