Preparation of carbon coated LiFePO4 by
β
Muxina Konarova; Izumi Taniguchi
π
Article
π
2009
π
Elsevier Science
π
English
β 963 KB
Carbon coated LiFePO 4 could be successfully prepared by a combination of spray pyrolysis (SP) with planetary ball-milling (BM) followed by heat treatment at 500 Β°C. SEM and TEM observations revealed that the carbon coated LiFePO 4 were much smaller in size than the bare LiFePO 4 prepared by the SP