๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Computer simulation of differential scanning calorimetry: influence of thermal resistance factors and simplex optimization of peak resolution

โœ Scribed by Jang, Guang Way.; Rajeshwar, Krishnan.


Book ID
125940253
Publisher
American Chemical Society
Year
1988
Tongue
English
Weight
769 KB
Volume
60
Category
Article
ISSN
0003-2700

No coin nor oath required. For personal study only.