Compression creep tests on niobium at high temperatures

✍ Scribed by G. Brinson


Book ID
118926412
Publisher
Elsevier Science
Year
1960
Weight
479 KB
Volume
2
Category
Article
ISSN
0022-5088

No coin nor oath required. For personal study only.


πŸ“œ SIMILAR VOLUMES


Creep of niobium at low temperatures
✍ G.A Stone; H Conrad πŸ“‚ Article πŸ“… 1964 πŸ› Elsevier Science βš– 534 KB

The activation energy, H, the activation volume, w\*, and the frequency factor, Y, for the plastic deformation of niobium at low temperatures (T < 0.2 T,) were derived from creep tests. The values of H and e\* for r\* = 1 kg/mm2 were 0.75 eV and 47bS respectively, decreasing with increase in stress.