Composition limits of the shape memory γ-phase in the system Fe-Mn-Al-Si
✍ Scribed by M.A. Peters; H.W. King
- Book ID
- 114008000
- Publisher
- Canadian Institute of Mining, Metallurgy and Petroleum
- Year
- 1997
- Tongue
- English
- Weight
- 524 KB
- Volume
- 36
- Category
- Article
- ISSN
- 0008-4433
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
The structure of a Cu-13.67Al-4.28Ni-0.54Mn-0.14Fe (wt.%) shape memory alloy was analyzed in the initial condition, during a heating-cooling cycle, and during a room temperature loading-unloading mechanical cycle. A fully reversible martensitic transformation was revealed which was associated with a
Fe-Mn-Si is a well-characterized ternary shape memory alloy. Research on this alloy has consistently shown that the addition of 5-6 wt.% Si is desirable to enhance the reversibility of stress-induced martensite vis-a `-vis shape memory. This paper examines the effect of Si on the morphology and the