Microstructural Evolution with a Wide Ra
Microstructural Evolution with a Wide Range of Solidification Cooling Rates in a Ni-Based Superalloy
โ
Yongjun Zhang, Bin Huang, Jianguo Li
๐
Article
๐
2013
๐
The Minerals, Metals & Materials Society
๐
English
โ 518 KB