✦ LIBER ✦
Combination of Nanoindentation and Quantitative Backscattered Electron Imaging Revealed Altered Bone Material Properties Associated with Femoral Neck Fragility
✍ Scribed by N. Fratzl-Zelman; P. Roschger; A. Gourrier; M. Weber; B. M. Misof; N. Loveridge; J. Reeve; K. Klaushofer; P. Fratzl
- Book ID
- 105913777
- Publisher
- Springer
- Year
- 2009
- Tongue
- English
- Weight
- 371 KB
- Volume
- 85
- Category
- Article
- ISSN
- 1432-0827