Coarsening of Al3Sc precipitates in an Al-0.28 wt pct Sc alloy
β Scribed by C. Watanabe; T. Kondo; R. Monzen
- Book ID
- 107440620
- Publisher
- The Minerals, Metals & Materials Society
- Year
- 2004
- Tongue
- English
- Weight
- 194 KB
- Volume
- 35
- Category
- Article
- ISSN
- 1073-5623
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
The yield stress and work hardening behaviour of precipitation hardening alloys is directly related to the nature of the interaction between mobile dislocations and precipitates. In commercial systems such as aluminium alloys, the understanding of this problem is complicated by the overlap between v
Dispersoids are usually formed during precipitation annealing (homogenisation) of aluminium alloys in order to inhibit recrystallisation during subsequent processing and/or use at high temperatures. In this respect, Al 3 (Sc x ,Zr 1-x )-dispersoids are most efficient, as they display the unique comb