Isotropic pitch-based carbon fibres are activated by carbon dioxide and by steam at a temperature ranging from 850 to IOOO'C. In both cases, a significant increase in micropore volume, as measured by physical adsorption of N, and COZ. is found. Fibre diameter steadily decreases during gasification b
Mesophase pitch-based carbon fibres thermoset with CI2 containing air were studied for their microstructures and physical properties. Carbon fibres thermoset with CI2 containing air and heat-treated at 2000 ~ (CI22000) possessed slightly smaller mean sizes of crystallites Lc(0 0 2)s, lower densities