Various unsaturated polyfunctional monomers were kneaded into cis-1,4polyisoprene containing fillers under 80ЊC and then irradiated using an electron beam accelerator to prepare vulcanized rubber with good quality. Results showed that 2G (diethyleneglycol dimethacrylate) is the best sensitizer. The
Clay nanolayer reinforcement of cis-1,4-polyisoprene and epoxidized natural rubber
✍ Scribed by Yen T. Vu; James E. Mark; Ly H. Pham; Martin Engelhardt
- Publisher
- John Wiley and Sons
- Year
- 2001
- Tongue
- English
- Weight
- 253 KB
- Volume
- 82
- Category
- Article
- ISSN
- 0021-8995
- DOI
- 10.1002/app.1976
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
## Abstract Telechelic __cis__‐1,4‐oligoisoprenes were prepared by the selective cleavage of weak epoxidized units (E) in epoxidized __cis__‐1,4‐polyisoprenes (EPIs) and by the random cleavage of isoprenic units (I) in __cis__‐1,4‐polyisoprene (PI). In both cases, cleavage by periodic acid (H~5~IO~
## Abstract In the presence of chlorinated solvents, the catalytic complex [Ir(COD)py(PCy~3~)]PF~6~ (where COD is 1,5‐cyclooctadiene and py is pyridine) was an active catalyst for the hydrogenation of synthetic __cis__‐1,4‐polyisoprene and natural rubber. Detailed kinetic and mechanistic studies fo