Chronoamperometric studies of pitting corrosion of Al and (Al–Si) alloys by halide ions in neutral sulphate solutions

✍ Scribed by Sayed S Abdel Rehim; Hamdi H Hassan; Mohammed A Amin


Book ID
116384089
Publisher
Elsevier Science
Year
2004
Tongue
English
Weight
374 KB
Volume
46
Category
Article
ISSN
0010-938X

No coin nor oath required. For personal study only.


📜 SIMILAR VOLUMES


Pitting Corrosion of Some α-Brasses in N
✍ Dr. H. A. Abd El-Rahman 📂 Article 📅 1990 🏛 John Wiley and Sons 🌐 English ⚖ 470 KB

## Abstract The pitting corrosion behaviour of some α‐brasses (Cu%: 85, 70, 67, 63 and 60) in neutral and alkaline solution containing various halide ions was studied. The pitting corrosion resulted in dezincification in all cases and the pitting potential was found with few exceptions to increase

Corrosion and passivation of Al and Al-S
✍ Faiza M. Al-Kharafi; Waheed A. Badawy 📂 Article 📅 1995 🏛 Elsevier Science 🌐 English ⚖ 638 KB

The electrochemical behaviour of aluminium and Al-silicon alloys in aqueous solutions containing different concentrations of chloride ions was investigated. Electrochemical impedance spectroscopy (EIS) and polarization techniques were used. The electrodes were anodically passivated under galvanostat

Pitting and repassivation processes of A
✍ P.L. Cabot; F.A. Centellas; E. Pérez; R. Loukili 📂 Article 📅 1993 🏛 Elsevier Science 🌐 English ⚖ 547 KB

Almtraet--The mechanism of localized corrosion of AI-5.03%Zn-l.67%Mg--0.23%Cu alloy submitted to different heat treatments (annealed (A); cold-rolled (ST); quenched (F); quenched and aged (13); and quenched in two stages and aged ((2)) in NaCI, NaaSO 4 and in NaCI-Na2SO 4 solutions has been studied