In compositions having ZrO2/Y203 = (74.25-71.25)/(0.75-3.75) (mol % ratio) with 25 mol % AI203, metastable t-Zr02 solid solutions crystallize at ~ 780 ~ to ~ 860 ~ from amorphous materials prepared by the simultaneous hydrolysis of zirconium, yttrium and aluminium acetylacetonates. Hot isostatic pre
✦ LIBER ✦
Change of tetragonal ZrO2content in ZrO2-toughened Al2O3by hot isostatic pressing
✍ Scribed by Saburo Hori; Masahiro Yoshimura; Shigeyuki Sōmiya; Hisatsugu Kaji
- Publisher
- Springer
- Year
- 1984
- Tongue
- English
- Weight
- 406 KB
- Volume
- 3
- Category
- Article
- ISSN
- 0261-8028
No coin nor oath required. For personal study only.
📜 SIMILAR VOLUMES
Hot isostatic pressing of tetragonal ZrO
✍
H. Watanabe; K. Hirota; O. Yamaguchi; S. Inamura; H. Miyamoto; N. Shiokawa; K. T
📂
Article
📅
1994
🏛
Springer
🌐
English
⚖ 814 KB
Formation of tetragonal ZrO2-glass struc
✍
R. McPherson
📂
Article
📅
1987
🏛
Springer
🌐
English
⚖ 180 KB
Fabrication and mechanical properties of
✍
K. Okuda; K. Shibata; M. Yoshinaka; K. Hirota; O. Yamaguchi
📂
Article
📅
1996
🏛
Springer
🌐
English
⚖ 753 KB
Characteristics of hot-pressed Al2O3chop
✍
K. Park; T. Vasilos
📂
Article
📅
1996
🏛
Springer
🌐
English
⚖ 348 KB
The role of tetragonal and monoclinic Zr
✍
Tomaž Kosmač; Michel V Swain; Nils Claussen
📂
Article
📅
1985
🏛
Elsevier Science
⚖ 609 KB
Transformed Zro2 volume fraction in Al2o
✍
Koji Ikeda; Teruo Kishi
📂
Article
📅
1991
🏛
Elsevier Science
🌐
English
⚖ 701 KB
AlsO3 matrix composites multi-toughened with Sic whiskers and ZrO, particles are used to obtain information about what happens in multi-toughened composites. By the help of Raman microspectroscopy and scanning electron microscopy, the following characteristics are revealed: (1) the stability of tetr