Catalytic effect in the hydrogenation of Mg and Mg compounds: Surface analysis of MgMg2Ni and Mg2Ni

✍ Scribed by L. Schlapbach; D. Shaltiel; P. Oelhafen


Book ID
113185708
Publisher
Elsevier Science
Year
1979
Tongue
English
Weight
618 KB
Volume
14
Category
Article
ISSN
0025-5408