𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Case study of failure in a glass-sealed SiC/SiC-based composite creep tested at 1100°C in air

✍ Scribed by Ian J. Davies; Toshio Ogasawara; Takashi Ishikawa; Naoto Suzuki


Book ID
117356222
Publisher
Elsevier Science
Year
2001
Tongue
English
Weight
317 KB
Volume
48
Category
Article
ISSN
0167-577X