An investigation of sc windings under mechanical loading showed that at and below liquid nitrogen temperature their deformation had a serrated character. Heat generation at some serrations can result in sc windings quench.
Calculation of the winding configuration of superconducting magnets
β Scribed by B.N. Zhurkov; V.N. Lebedev; I.A. Mozalevskii
- Publisher
- Elsevier Science
- Year
- 1976
- Tongue
- English
- Weight
- 359 KB
- Volume
- 16
- Category
- Article
- ISSN
- 0011-2275
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
The influence of the volume of the superconducting winding interlayer space and the structure of the insulation coating upon the conductor recovery current value Ir has been investigated experimentally. An analysis of the optimum conductor insulation coating was performed, considering different form
A simple qualitative model is proposed to explain the fast initial change of the magnetic field of superconducting magnets which operate in the persistent mode. Using this model the additional component of the transport current which is induced by the decaying screening currents can be represented.