Calculation of superalloy phase diagrams: Part IV

✍ Scribed by Kaufman, Larry ;Nesor, Harvey


Book ID
113000751
Publisher
The Minerals, Metals & Materials Society
Year
1975
Tongue
English
Weight
965 KB
Volume
6
Category
Article
ISSN
1543-1916