Sol-gel-derived SiO 2 and CaO-P 2 O 5 -SiO 2 have been shown to be bioactive and bone bonding. In this study bioactive sol-gel-derived SiO 2 and CaO-P 2 O 5 -SiO 2 systems were tested for in in vitro bioactivity. The calcined ceramic monoliths were immersed in a simulated body fluid and analyzed to
Calcium phosphate formation on sol-gel-derived bioactive glassesin vitro
β Scribed by Pereira, M. M. ;Clark, A. E. ;Hench, L. L.
- Book ID
- 111700549
- Publisher
- John Wiley and Sons
- Year
- 1994
- Tongue
- English
- Weight
- 427 KB
- Volume
- 28
- Category
- Article
- ISSN
- 0021-9304
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Titanium and its alloys have been used successfully in the manufacture of orthopedic and dental implants to replace damaged bone tissue. In this study, different solgel-derived TiO 2 coatings were produced on titanium substrates using different aging times (5, 10, 24, or 48 h) of the sol before dipp
Titanium and its alloys are used widely in the manufacture of orthopedic and dental implants. Sol-gelprepared titania is able to stimulate bone-like apatite formation in in vitro and in vivo cultures. These materials can be used, for example, as coatings on dental and orthopedic implants. However, t
Calcium phosphate formation is induced within sol-gel prepared titania and grows toward a calcium phosphate solution in which the titania is immersed. The implantation of this sol-gel prepared titania film coating on TiA16V4 core into the femurs of goats shows an accumulation of calcium phosphate wi
A glass with a composition of SiO 2 80% and CaO 20% (in mol %) was prepared by the sol-gel method, and its in vitro bioactivity was studied by soaking it in simulated body fluid (SBF) at 37Β°C. The formation of a calcium phosphate layer on the glass was analyzed by determining the ionic concentration