Bioactive glass as precursor of designed-architecture scaffolds for tissue engineering

✍ Scribed by S. Padilla; S. Sánchez-Salcedo; M. Vallet-Regí


Publisher
John Wiley and Sons
Year
2007
Tongue
English
Weight
676 KB
Volume
81A
Category
Article
ISSN
1549-3296

No coin nor oath required. For personal study only.

✦ Synopsis


Abstract

In this work, the conditions to obtain concentrated and fluid suspensions from a bioactive glass (55‐SiO~2~; 41‐CaO; 4‐P~2~O~5~; mol %) were investigated. The influence of the heat treatment of the glass on the specific surface area, solubility, bioactivity, and finally on their dispersion characteristics was studied. Zeta potential and viscosity measurements were carried out, and based on the obtained results, the best dispersant was selected. The optimum concentration of dispersant, maximum content of solid and time of mixing were also investigated. Slurries containing 50 vol % could be obtained calcining the glass at 1100°C and using Darvan 811 (sodium polyacrylate) as dispersant. Scaffolds with designed architecture were prepared from these suspensions combining the gelcasting method and the stereolithography technique. A polymeric negative (replica of the desired structure) was previously obtained by stereolithography. The slurry was cast into the molds and then polymerized (gelcasting method). The negative was eliminated by heat treatment. After sintering at 1300°C, scaffolds with interconnected porosity and three‐dimensional channels of 400–470 μm and macropores of 1.4 μm were obtained. © 2006 Wiley Periodicals, Inc. J Biomed Mater Res 2007


📜 SIMILAR VOLUMES


Sol–gel synthesis of bioactive glass sca
✍ Marlene de Barros Coelho; Marivalda Magalhães Pereira 📂 Article 📅 2005 🏛 John Wiley and Sons 🌐 English ⚖ 207 KB 👁 1 views

## Abstract Well‐defined structural characteristics are some of the exigencies that have to be attended when scaffolds for bone tissue cell culture are designed. A high porosity (70–90%) and a high specific surface area and an average pore size > 150 μm will contribute to allow cell migration throu

Polylactic acid–phosphate glass composit
✍ G. Georgiou; L. Mathieu; D. P. Pioletti; P.-E. Bourban; J.-A. E. Månson; J. C. K 📂 Article 📅 2007 🏛 John Wiley and Sons 🌐 English ⚖ 483 KB

## Abstract Phosphate glass (PG) of the composition 0.46(CaO)–0.04(Na~2~O)–0.5(P~2~O~5~) was used as filler in poly‐L‐lactic acid (PLA) foams developed as degradable scaffolds for bone tissue engineering. The effect of PG on PLA was assessed both in bulk and porous composite foams. Composites with

Crosslinked poly(ϵ-caprolactone/D,L-lact
✍ V.V. Meretoja; A.O. Helminen; J.J. Korventausta; V. Haapa-aho; J.V. Seppälä; T.O 📂 Article 📅 2006 🏛 John Wiley and Sons 🌐 English ⚖ 246 KB

## Abstract A series of elastic polymer and composite scaffolds for bone tissue engineering applications were designed. Two crosslinked copolymer matrices with 90/10 and 30/70 mol % of ϵ‐caprolactone (CL) and D,L‐lactide (DLLA) were prepared with porosities from 45 to 85 vol % and their mechanical

Factors affecting the structure and prop
✍ Jones, Julian R. ;Hench, Larry L. 📂 Article 📅 2003 🏛 John Wiley and Sons 🌐 English ⚖ 275 KB 👁 1 views

## Abstract Resorbable 3D macroporous bioactive scaffolds have been produced for tissue‐engineering applications by foaming sol‐gel–derived bioactive glasses of the 58S (60 mol% SiO~2~, 36 mol% CaO, 4 mol% P~2~O~5~) composition with the aid of a surfactant. Bioactive glasses are known to have the a

Design and characterization of a biodegr
✍ James W. S. Hayami; Denver C. Surrao; Stephen D. Waldman; Brian G. Amsden 📂 Article 📅 2009 🏛 John Wiley and Sons 🌐 English ⚖ 548 KB

## Abstract Herein we report on the development and characterization of a biodegradable composite scaffold for ligament tissue engineering based on the fundamental morphological features of the native ligament. An aligned fibrous component was used to mimic the fibrous collagen network and a hydrog