Measurement of the local mechanical prop
✍ Siddhartha Pathak; Dejan Stojakovic; Surya R. Kalidindi πŸ“‚ Article πŸ“… 2009 πŸ› Elsevier Science 🌐 English βš– 725 KB

This paper describes the development of novel experimental protocols and data analysis procedures for extracting meaningful indentation stress-strain curves from spherical nanoindentation on polycrystalline samples, and correlating these measurements to the local crystal lattice orientation measured