𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Behavior of nickel-base superalloy single crystals under thermal-mechanical fatigue: Fleury, E. and Remy, L. Metall. Trans. A (Jan. 1994) 25A(1), 99–109


Publisher
Elsevier Science
Year
1994
Tongue
English
Weight
165 KB
Volume
16
Category
Article
ISSN
0142-1123

No coin nor oath required. For personal study only.