An original lead-acid battery structure incorporating a special set of separators and a device to exert mechanical pressure on the plates is described. An additional arrangement on the positive plates reduces shedding. Such batteries were cycled using thirty minute rapid charges, and cycle lives of
BCI cycle life testing procedures for deep-cycle lead-acid batteries
β Scribed by G. Mayer
- Publisher
- Elsevier Science
- Year
- 1986
- Tongue
- English
- Weight
- 28 KB
- Volume
- 17
- Category
- Article
- ISSN
- 0378-7753
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
## Several characteristics of the well-known lead/acid battery can be improved by developing valve-regulated units (VRLAS) with absorptive glass mat (AGM) separators. In spite of the fact that antimony-free alloys are used, very good cycle-life is achieved. The performance of conventional flooded
Optimized designs for advanced lead-acid, load-leveling batteries were selected in a limited time period by means of an accelerated life cycle test combining two 80% D.O.D. cycles per day with a target mean test temperature of 71 "C. Preprototype load-leveling cell designs were selected from 60 cell