✦ Synopsis


The degradable polymers poly(orthoester) (POE), poly(Llactic acid) (PLA), and the nondegradable polymers polysulfone (PSF), polyethylene (PE), and poly(ether ether ketone) (PEEK) were exposed to cultures of Staphylococcus epidermidis, Pseudomonas aeruginosa, or Esckerichia coli. Bacteria washed and resuspended in phosphate buffered saline (PBS) adhered to polymers in amounts nearly twice those of bacteria that were left in their growth medium, tryptic soy broth (TSB). In TSB, there was variation in adhesion from species to species, but no significant variation from polymer to polymer within one species. In PBS there were significant differences in the amounts of bacteria ad-hering to the various polymers with the exception of s.

epidermidis, which had similar adhesion to all polymers. As a whole, P. aeruginosa was the most adherent while S. epidermidis was the least adherent. The estimated values of the free energy of adhesion (AF,,,) correlated with the amount of adherent P. aeruginosa. When POE, PLA, and PSF were exposed to hyaluronic acid (HA) before exposure to the bacteria, there was 50% more adhesion of E. coli and P. aeruginosa on POE and PLA. With respect to bacterial adhesion, the biodegradable polymers (POE and PLA) in general were not significantly different from the nondegradable polymers.


πŸ“œ SIMILAR VOLUMES


Better osteoblast adhesion on nanopartic
✍ Venu Perla; Thomas J. Webster πŸ“‚ Article πŸ“… 2005 πŸ› John Wiley and Sons 🌐 English βš– 645 KB

## Abstract Apart from problems such as poor osseointegration, stress shielding, and wear debris‐associated bone cell death, a major concern of metallic orthopedic implants is that they slowly corrode under __in vivo__ environments. It is possible that continuous tissue exposure to metallic corrosi

Toxicity measurement of orthopedic impla
✍ Shettlemore, Melissa G. ;Bundy, Kirk J. πŸ“‚ Article πŸ“… 1999 πŸ› John Wiley and Sons 🌐 English βš– 268 KB

The toxicity of aqueous metal solutions representative of ionic degradation products from orthopedic implant alloys was determined using a bacterial bioluminescence assay, Microtox. The toxicity of forms of the individual elements released from ASTM F75 Co-Cr-Mo (Co-Cr-Mo), F138 316L stainless steel

Bioactive hydroxyapatite coatings on pol
✍ C. Auclair-Daigle; M. N. Bureau; J.-G. Legoux; L'H. Yahia πŸ“‚ Article πŸ“… 2005 πŸ› John Wiley and Sons 🌐 English βš– 607 KB

## Abstract Hydroxyapatite [HA, Ca~10~(PO~4~)~6~(OH)~2~] coatings on polymer composite substrates were investigated for their bioactivity and their physicochemical and mechanical characteristics. HA holds key characteristics for use in orthopedic applications, such as for coating of the femoral ste