Automatic recognition of welding defects in real-time radiography

โœ Scribed by Duguid, J.B.; Robertson, W.B.


Book ID
122404248
Publisher
Elsevier Science
Year
1991
Tongue
English
Weight
159 KB
Volume
24
Category
Article
ISSN
0963-8695

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Automatic recognition of welding defects
๐Ÿ“‚ Article ๐Ÿ“… 1996 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 186 KB

## Reliability of non-destructive examination of welded joints Dept. Civil engineering, Imperial College London, CESLIC Report OR7,74 pp. (Feb. 1989) This report reviews published information from several national and international programmes on detection probabilities and sizing errors. Currently