Assessment of welding defects for gas pi
โ
H.I. Shafeek; E.S. Gadelmawla; A.A. Abdel-Shafy; I.M. Elewa
๐
Article
๐
2004
๐
Elsevier Science
๐
English
โ 652 KB
In this paper, a novel automated vision system is introduced to detect and assess the welding defects of gas pipelines from the radiographic films. The proposed vision system was used to capture images for the radiographic films and apply various image processing and computer vision algorithms to de