𝔖 Bobbio Scriptorium
✦   LIBER   ✦

Atomic ordering in the phases of a nickel-chromium-based superalloy

✍ Scribed by V. I. Goman’kov; G. I. Nosova; V. V. Rtishchev; S. E. Manaenkov; L. E. Fykin


Book ID
110186982
Publisher
SP MAIK Nauka/Interperiodica
Year
2008
Tongue
English
Weight
239 KB
Volume
2008
Category
Article
ISSN
0036-0295

No coin nor oath required. For personal study only.