๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Approaches to the lowest core loss in grain-oriented 3% silicon steel with high permeability

โœ Scribed by Sato, T.; Kuroki, K.; Tanaka, O.


Book ID
117923561
Publisher
IEEE
Year
1978
Tongue
English
Weight
409 KB
Volume
14
Category
Article
ISSN
0018-9464

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Study of vacuum levels in the annealing
โœ I. Ibarrondo; J. Degauque ๐Ÿ“‚ Article ๐Ÿ“… 1999 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 90 KB

In the present study, high silicon (6.4 wt%) -iron microcrystalline ribbons (25 mm;38 m) were obtained directly from its melted state by rapid quenching. The material thus obtained was then submitted to heat treatment. This soft magnetic material is mainly used as cores in high-performance electric