๐”– Bobbio Scriptorium
โœฆ   LIBER   โœฆ

Application of Monte Carlo simulation for fractographic analysis of fatigue crack propagation

โœ Scribed by T. Shimokawa; Y. Kakuta


Publisher
Elsevier Science
Year
1996
Tongue
English
Weight
707 KB
Volume
18
Category
Article
ISSN
0142-1123

No coin nor oath required. For personal study only.


๐Ÿ“œ SIMILAR VOLUMES


Application of Macro Response Monte Carl
โœ L.A. Perles; A. de Almeida ๐Ÿ“‚ Article ๐Ÿ“… 2007 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 200 KB

During the past years several variance reduction techniques for Monte Carlo electron transport have been developed in order to reduce the electron computation time transport for absorbed dose distribution. We have implemented the Macro Response Monte Carlo (MRMC) method to evaluate the electron spec

Monte-Carlo simulation of complex vapor-
โœ Y. Zhang; G.D. Alton ๐Ÿ“‚ Article ๐Ÿ“… 2005 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 223 KB

In order to minimize decay losses of short-lived radioactive species at ISOL based RIB facilities, effusive-flow particle transit times between target and ion source must be as short as practically achievable. A Monte-Carlo code has been developed for simulating the effusive-flow of neutral particle

Errors Associated with Metabolic Control
โœ Edward K. Ainscow; Martin D. Brand ๐Ÿ“‚ Article ๐Ÿ“… 1998 ๐Ÿ› Elsevier Science ๐ŸŒ English โš– 188 KB

The errors associated with experimental application of metabolic control analysis are difficult to assess. In this paper, we give examples where Monte-Carlo simulations of published experimental data are used in error analysis. Data was simulated according to the mean and error obtained from experim