## Abstract Superplastic forming limit diagrams (SPFLDs) are presented for both Tiβ6Alβ4V and Tiβ6Alβ2Snβ4Zrβ2Mo alloys. FEβpredicted __Ο΅__~1~β__Ο΅__~3~βΟ΅~__eq__~ paths for key points on the forming blank are then plotted on the SPFLD to predict failure. A key factor for reliable SPF forming limit p