The mechanism of the thermal degradation of polystyrene was studied by pyrolysis-gas chromatography and pyrolysis-field ionization mass spectrometry, using a block copolymer of ordinary and perdeuterated styrene [poly(styrene-b-styrene-ds) ]. The main degradation products were monomers, dimers and t
Analysis by pyrolysis/gas chromatography/mass spectrometry of glass fibre/vinylester thermal degradation products
โ Scribed by N. Regnier; B. Mortaigne
- Publisher
- Elsevier Science
- Year
- 1995
- Tongue
- English
- Weight
- 909 KB
- Volume
- 49
- Category
- Article
- ISSN
- 0141-3910
No coin nor oath required. For personal study only.
๐ SIMILAR VOLUMES
Analytical pyrolysis methods were applied to the study of evolution of chlorinated thermal decomposition products from organic plastics pigments. The identification of the organic volatile compounds was performed by fast pyrolysis-gas chromatography/mass spectrometry. In addition, temperature progra
## Abstract A series of poly(acyl sulfides) were synthesized by polycondensation of acid dichlorides with sodium sulfide using tetrabutylammoniumhydrogen sulfate as a phase transfer catalyst. The thermal stability of these polymers was determined by thermogravimetric analysis. A unique phenomenon o
Flash-pyrolyses of two furfuraldehyde resins were performed at 980 and 770 ยฐ. The identities of volatile products were established by employing two coupled systems, viz. pyrolysis(gas chromatography)-(mass spectrometry) in electron-impact and chemical-ionization modes and pyrolysis(gas chromatograph
A mass spectrometric investigation has been performed on the gases evolved during the pyrolysis of natural and some synthetic rubbers over the temperature range 30-4500 It was found that variations in ion ratio with temperature reveal interesting structural information. The ion ratiotemperature prof