Samples of P33 carbon black, heat treated in the range 1600"-26OO"C, were studied by E.P.R. The lineintensity, localized and free spins contributions, and g-factor, are examined as a function of residence time at H.T.T. (a few minutes to several hours). The correlation between the g-factor and diama
An electron spin resonance investigation of carbon black-filled polybutadiene
β Scribed by E. M. Cashell; V. J. McBrierty
- Publisher
- Springer
- Year
- 1977
- Tongue
- English
- Weight
- 664 KB
- Volume
- 12
- Category
- Article
- ISSN
- 0022-2461
No coin nor oath required. For personal study only.
π SIMILAR VOLUMES
Electrochemical reduction of either of two different carbon blacks dispersed in methylene chloride gave rise to a temperature independent narrow ESR signal superimposed upon the characteristic broad signal. The observation of this conduction ESR (CESR) signal implies that there are two distinct envi
## Abstract This work investigates the behaviour of elastomeric chains (polybutadienes of identical molecular weight but different microstructures) in the close vicinity of carbon black surfaces in order to attain a better understanding of the structure and properties of interphases. Elastomerβfill